Ubwiza Bwiza Ton ya Invar Permalloy Inconel 625 718 Ni80cr20 Monel Incoloy Yera Nickel Superalloy Isahani Icyuma Nickel Alloy Sheet
Ibisobanuro bigufi:
Inconel625 alloy (UNS 6625) ni austenitis superheat irwanya amavuta cyane cyane igizwe na nikel, ifite imiterere myiza yo kurwanya okiside nini no kurwanya ruswa.
Turakomeza dukurikiza ihame ry "ubuziranenge bwambere, serivisi mbere yambere, iterambere rihoraho no guhanga udushya kugirango duhure nabakiriya" kubuyobozi na "inenge zeru, ibibazo bya zeru" nkintego nziza.Kugirango dushyigikire ubufasha bwacu, dutanga ibicuruzwa mugihe dukoresha ubuziranenge buhebuje ku giciro cyiza cya Toni nziza ya Invar Permalloy Inconel 625 718 Ni80cr20 Monel Incoloy Yera Nickel Superalloy Plate Icyuma Nickel Alloy Sheet, Nkuruganda rukomeye kandi rwohereza ibicuruzwa hanze, twe kwishimira izina ryiza kumasoko mpuzamahanga, cyane cyane muri Amerika no muburayi, kubera ubuziranenge bwacu kandi nibiciro byiza.
Turakomeza dukurikiza ihame ry "ubuziranenge bwambere, serivisi mbere yambere, iterambere rihoraho no guhanga udushya kugirango duhure nabakiriya" kubuyobozi na "inenge zeru, ibibazo bya zeru" nkintego nziza.Kugira ngo ubufasha bwacu butangwe, dutanga ibicuruzwa mugihe dukoresha ubuziranenge buhebuje ku giciro cyiza kuriUbushinwa Nickel Alloy Isahani hamwe nisahani, burigihe duhorana inguzanyo hamwe ninyungu kubakiriya bacu, dushimangira serivise nziza yo kwimura abakiriya bacu.burigihe twakira inshuti zacu nabakiriya bacu kuza gusura isosiyete yacu no kuyobora ubucuruzi bwacu, niba ushimishijwe nibicuruzwa byacu, urashobora kandi gutanga amakuru yubuguzi kumurongo, kandi tuzahita tuvugana nawe, dukomeze ubufatanye buvuye kumutima kandi tubifuriza ibintu byose muruhande rwawe byose ni byiza.
Inconel625 alloy (UNS 6625) ni austenitis superheat irwanya amavuta cyane cyane igizwe na nikel, ifite imiterere myiza yo kurwanya okiside nini no kurwanya ruswa.Irakwiriye mubice byinshi birimo moteri yindege ibidukikije, indege, no gutunganya imiti.Ku bushyuhe buri munsi ya dogere 2000 Fahrenheit (dogere selisiyusi 1093), iyi mavuta nayo irerekana umunaniro udasanzwe.Imbaraga za 625 alloy zituruka ku ngaruka zikomeye za molybdenum na niobium ibisubizo bikomeye bikubiye muri nikel chromium alloy.Ibi bintu kandi bitanga umusemburo mwiza wo kurwanya ruswa.Nubwo iyi mavuta yagenewe imbaraga mubushyuhe bwo hejuru, ubushyuhe bwayo buvanze butanga kwihanganira cyane kwangirika kwinshi hamwe nuburyo butandukanye bwa okiside hamwe n’ibidukikije.Chromium hamwe na molybdenum biha amavuta imbaraga zo kurwanya ibibora byangirika biterwa na chloride ion ziranga: Nikel nyinshi yongerera imbaraga imbaraga zo kurwanya amavuta ya chloride.
ASTM B443 / ASME SB-443 、 ASTM B444 / ASME SB-444 、 ASTM B366 / ASME SB-366 、 ASTM B446 / ASME SB-446 、 ASTM B564 / ASME SB-564
C | Mn | Ni | Si | P | Cr | S | Fe | Al | Ti | Nb | Co | Mo |
≤0.01 | ≤0.50 | ≥58 | ≤0.50 | ≤0.015 | 20.0 ~ 23.0 | ≤0.015 | ≤5.0 | ≤0.4 | ≤0.4 | 3.15 ~ 4.15 | ≤1.0 | 8.0 ~ 10.0 |
Ubucucike | Ingingo yo gushonga |
8.44g / cm3 | 1290-1350 ℃ |
Imbaraga | Gutanga Imbaraga | Kurambura | Gukomera |
σb≥758Mpa | σb≥379Mpa | δ≥30% | HB150-220 |
ERNiCrMo-3 ENiCrMo-3
Gutanga ibicuruzwa
Isahani, Ikibaho, Akabari, Umugozi, Guhimba, Inkoni yoroshye, ibikoresho byo gusudira, Flange, nibindi. Turashobora kandi gutunganywa dukurikije igishushanyo
Ibigize imiti mvaruganda irimo chloride, cyane cyane iyo ukoresheje aside ya chloride acide;Ibigega byo guteka no guhumeka bikoreshwa munganda nimpapuro;Umunara winjiza, reheater, flue gas inlet baffle, umuyaga (wet), agitator, isahani yo kuyobora, hamwe na flue muri sisitemu ya gazi ya disulfurizasi;Ikoreshwa mugukora ibikoresho nibikoresho byo gukoresha mubidukikije bya gaze acide;Acide acetike na acide anhydride itanga amashanyarazi;Umuyoboro wa aside ya sulfuru;Ibikoresho bya farumasi;Inganda nibicuruzwa nkibikoresho byo kwagura inzogera.
INCONEL 625 ni austenitis superheat irwanya amavuta cyane cyane igizwe na nikel.Bikomoka ku ngaruka zikomeye za molybdenum na niobium ibisubizo bikomeye bikubiye muri nikel chromium alloys, ifite imbaraga zidasanzwe kandi zirwanya umunaniro udasanzwe ku bushyuhe buke bugera kuri 1093 and, kandi ikoreshwa cyane mu nganda zindege.Nubwo iyi mavuta yagenewe imbaraga mubushyuhe bwubushyuhe bwo hejuru, ibiyirimo byinshi bya chromium na molybdenum bifite imbaraga nyinshi zo kurwanya itangazamakuru ryangirika, kuva ahantu hashobora kuba okiside cyane kugeza ahantu rusange rushobora kwangirika, hamwe no kurwanya ruswa cyane, bikerekana ruswa irwanya ruswa. ibiranga.INCONEL 625 ifite kandi imbaraga zo kurwanya ruswa kurwanya itangazamakuru ryanduye rya chloride nk'amazi yo mu nyanja, amazi ya geothermal, umunyu utabogamye, n'amazi y'umunyu.
Turakomeza dukurikiza ihame ry "ubuziranenge bwambere, serivisi mbere yambere, iterambere rihoraho no guhanga udushya kugirango duhure nabakiriya" kubuyobozi na "inenge zeru, ibibazo bya zeru" nkintego nziza.Kugirango dushyigikire ubufasha bwacu, dutanga ibicuruzwa mugihe dukoresha ubuziranenge buhebuje ku giciro cyiza cya Toni nziza ya Invar Permalloy Inconel 625 718 Ni80cr20 Monel Incoloy Yera Nickel Superalloy Plate Icyuma Nickel Alloy Sheet, Nkuruganda rukomeye kandi rwohereza ibicuruzwa hanze, twe kwishimira izina ryiza kumasoko mpuzamahanga, cyane cyane muri Amerika no muburayi, kubera ubuziranenge bwacu kandi nibiciro byiza.
UbwizaUbushinwa Nickel Alloy Isahani hamwe nisahani, burigihe duhorana inguzanyo hamwe ninyungu kubakiriya bacu, dushimangira serivise nziza yo kwimura abakiriya bacu.burigihe twakira inshuti zacu nabakiriya bacu kuza gusura isosiyete yacu no kuyobora ubucuruzi bwacu, niba ushimishijwe nibicuruzwa byacu, urashobora kandi gutanga amakuru yubuguzi kumurongo, kandi tuzahita tuvugana nawe, dukomeze ubufatanye buvuye kumutima kandi tubifuriza ibintu byose muruhande rwawe byose ni byiza.